Materials · nickel superalloys
Inconel 625 and 718: what they’re for, machining and cutting nickel superalloys
Why Inconel is so hard to machine (work hardening, heat, abrasion), differences between 625 and 718 (age-hardenable), carbide and ceramic tooling strategy, and waterjet, laser or plasma cutting.
“Inconel” is a brand (Special Metals) that became the common name for nickel-based superalloys. They keep their strength at high temperature and resist corrosion — exactly what makes them hard to machine: heat stays in the tool, the material work-hardens and it’s abrasive.
625 vs 718
| Criterion | Alloy 625 (UNS N06625) | Alloy 718 (UNS N07718) |
|---|---|---|
| Hardening | Solid-solution strengthened (no aging) | Age-hardenable (precipitation) |
| Strengths | Corrosion, weldability, fatigue | Very high strength up to high temperature |
| Typical uses | Chemical, marine, cladding, bellows | Aerospace (discs, shafts, fasteners), oil and gas |
| Machining | Difficult | Difficult; even more so after aging |
Machining strategy
- 718: rough and semi-finish in the solution-annealed condition, age, then finish lightly (Machining Doctor and tooling guides recommend avoiding heavy stock removal in the aged condition).
- Tools: sharp, positive coated carbide for finishing and for 625; ceramics (round, gradual entry) only for roughing in continuous cuts on a rigid machine, per Sandvik Coromant’s heat-resistant superalloy (HRSA) guide.
- Minimum chip thickness: never “stroke” the material; too light a feed work-hardens the surface and ruins the next tool.
- No dwelling in the cut, no re-cutting the work-hardened layer.
- Coolant in volume, high pressure if possible; very rigid setup.
- Speeds: well below stainless; follow the tool’s data (see Feeds and speeds) and track wear (see Tool life).
Cutting sheet and plate
| Process | Notes |
|---|---|
| Waterjet | Safest for quality: no heat-affected zone; see Waterjet |
| Fiber laser | Common on thin material with nitrogen, depending on machine and recipe |
| Plasma | Possible (“stainless/alloy” charts depending on the source), heat zone and edge to clean up |
| Saw / abrasive disc | Slow, high wear |
Common mistakes
| Mistake | Consequence |
|---|---|
| Stainless speeds | Tool destroyed in seconds |
| Feed too light “to be safe” | Work hardening, accelerated wear |
| Ceramics in interrupted cuts | Insert chipping |
| Roughing 718 that’s already aged | Cycle time and tooling cost multiplied |
Checklist
- Exact alloy and condition (625 annealed; 718 solution-treated or aged, AMS spec)
- Material certificate and traceability (often required in aerospace)
- Dedicated tools, new or in good condition; strategy proven on a test
- Allowance for finishing after aging (718)
- Price checked: nickel is expensive and volatile (see the price comparison tool)
FAQ
Is Inconel magnetic?
Alloys 625 and 718 are essentially non-magnetic at room temperature.
Can Inconel be replaced with 316 stainless?
Not without the designer’s approval: at high temperature or in very corrosive environments, 316 doesn’t offer the same properties.
Sources
- Sandvik Coromant — Heat resistant super alloys, application guide (PDF), consulted November 26, 2026.
- Machining Doctor — Machining Inconel: turning, milling and drilling guide, consulted November 26, 2026.
- American Machinist — Rx for high-nickel anxiety, consulted November 26, 2026.