Materials · stainless
Stainless steel in the shop: 303, 304 and 316, work hardening, machining, cutting and finish
303 for machining, 304 for general use, 316 for corrosion: differences, sheet finishes (2B, #4), work hardening and how to avoid it, nitrogen laser and plasma cutting, dedicated tools, linked to published prices.
Austenitic stainless 303, 304 and 316 cover most shop needs. They look alike, but not when machining or in corrosion. Their big shared trap: work hardening — stainless hardens under the tool if it rubs instead of cutting.
The three grades
| Grade | Distinctive feature | Use | In the shop |
|---|---|---|---|
| 303 | Added sulfur (inclusions that break the chip) | Production machined parts (bar) | Easiest to machine of the three; lower corrosion resistance and weldability; rare as sheet |
| 304 / 304L | Basic “18-8” stainless; L = low carbon for welding | Sheet, tube, food equipment, general use | Harder to machine (gummy, work-hardens) |
| 316 / 316L | Added molybdenum → better chloride resistance | Marine, chemical, pharma, road salt | A bit harder still than 304 to machine |
| 430 (ferritic) | Magnetic, no nickel | Appliances, decoration | Cheaper, lower corrosion resistance |
Parts makers quote machinability indexes of about 75–80% for 303, about 45% for 304 and 35–40% for 316 (free-machining steel reference): mostly remember the order 303 > 304 > 316.
Common sheet finishes
| Finish | Look | Use |
|---|---|---|
| 2B | Cold-rolled, matte-satin | General industrial use |
| #4 (brushed) | Grained, satin | Visible: counters, cladding |
| BA | Bright annealed | Decorative, reflective |
Order protective film if the face is visible, and specify grain direction for #4 parts.
Machining without work hardening
- Sharp positive-rake tools, coated carbide; change them before heavy wear.
- Firm, continuous feed: never let the tool rub or stop in the cut (no dwell).
- Cut below the work-hardened layer from the previous pass (enough depth).
- Rigid setup, generous coolant; moderate speeds per the tool’s data (see Feeds and speeds).
Cutting stainless
- Fiber laser with nitrogen: clean, oxide-free edge; a blued edge often means contaminated gas (see Laser: dross and burning).
- Plasma: stainless charts (air, or specific gases depending on the source, e.g. F5 or H35 on some systems); see Reading cut charts.
- No standard oxyfuel (see Oxyfuel cutting).
Avoiding contamination
- Tools, brushes, discs and tables dedicated to stainless, or protection (film, wood) on steel tables.
- Embedded iron particles rust and stain: cleaning and passivation per good practice if needed.
Common mistakes
| Mistake | Consequence |
|---|---|
| Choosing 303 for a welded part or salty environment | Inadequate weldability and corrosion resistance |
| Letting the tool rub | Work-hardened surface, burned tool |
| Same brushes as for steel | Contamination rust |
| 304 in chlorides (salt, pools) | Pitting; prefer 316 |
Ordering checklist
- Exact grade (304 vs 304L, 316 vs 316L)
- Finish (2B, #4, BA) and protective film
- Thickness as gauge and decimal (stainless table, see Sheet metal gauges)
- Mill certificate if required
- Compare published prices in the price comparison tool
FAQ
Is 304 stainless magnetic?
Annealed, barely; it can become slightly magnetic after cold work (bending, machining). It isn’t a reliable grade test.
Is 17-4PH stainless too?
Yes, a martensitic precipitation-hardening stainless, heat treated: see 17-4PH: conditions A, H900, H1150.
Sources
- Carpenter Technology — Ideas for machining austenitic stainless steels, consulted November 26, 2026.
- Wexmar — Machining 303, 304 and 316 stainless: work hardening, tooling and cost, consulted November 26, 2026.
- KGL Manufacturing — Stainless steel machinability: 303, 304, 316 and 17-4 PH compared, consulted November 26, 2026.