Process · before welding
Preparing parts for welding: bevels, root face, root opening and cleanliness
Groove joint vocabulary (angle, root face, root opening), where dimensions come from (welding procedure, CSA W59, AWS D1.1), how to cut and clean the bevel with plasma, oxyfuel or grinding, and a fit-up checklist.
A good weld starts at the cut. A poorly cut bevel, an uneven root face or an oxidized surface costs more in grinding, rework and rejects than careful machine setup.
Groove joint vocabulary
| Term | French | Definition |
|---|---|---|
| Bevel angle | Angle de chanfrein | Angle cut on one piece |
| Included angle / groove angle | Angle d’ouverture | Total angle between both pieces (two 30° bevels → 60°) |
| Root face / land | Talon | Unbevelled flat at the bottom of the joint |
| Root opening / gap | Écartement | Distance between the pieces at the root |
| V, double-V, U, J groove | Préparation en V, X, U, J | Joint shape based on thickness and access |
Example from a Lincoln Electric pipe welding guide: 60° included angle (30° per side), root face and root opening of about 1/16 in. That is a procedure example for one case, not a universal rule.
Cutting the bevel
| Method | Advantages | Limits |
|---|---|---|
| Plasma with bevel head (CNC) | Fast, repeatable, bevels built into the parts | Investment, angle compensation setup; see Plasma bevel cutting |
| Manual plasma or oxyfuel with a guide | Inexpensive | Consistency depends on the operator |
| Beveling machine (rotary, portable or stationary) | Clean machined surface, no heat zone | Speed, mostly straight edges |
| Grinding | Available everywhere | Slow, uneven, dust |
| Machining (mill, lathe) | Highest precision, exact land | Limited part size |
Clean before welding
- Mill scale, cutting oxide, rust, paint, oil: remove from the weld zone per the WPS (often a few centimetres each side).
- Edge cut with oxygen (laser or oxyfuel): oxide layer to consider per the procedure.
- Aluminum: dedicated stainless brush and degrease right before welding.
- Stainless: dedicated tools (brushes, discs) to avoid iron contamination.
- Remove dross and burrs (see Deburring and finishing).
Quebec shops offering this service
- SMF Mécanique (Services Mécanique Fabrication) Partner
Berthierville, QC
CNC machining (turning, milling, drilling, large parts), TIG/MIG/stick welding in shop or on site, custom fabrication and surface finishing.
smfmecanique.com (opens in a new tab) - Fabmec
Jonquière (Saguenay), QC
Industrial plasma cutting, including bevels for weld preparation.
fabmec.ca (opens in a new tab) - Nitek Laser
Nicolet, QC
Laser cutting and precision chamfering for welding.
niteklaser.com (opens in a new tab) - Québec Soudure
Québec, QC
Welding and metal fabrication.
quebecsoudure.com (opens in a new tab) - Soudure NT
Saint-Télesphore, QC
3000 W fiber laser (5 × 10 ft), 160-ton CNC bending and MIG/TIG welding.
soudurent.com (opens in a new tab)
Partner: a company linked to the CoupeFab team. The other shops are listed free of charge and in no order of preference. Services checked on each shop’s official website on November 26, 2026; confirm capacity and lead time before ordering.
Common mistakes
| Mistake | Consequence |
|---|---|
| Root face too thick | Lack of root penetration |
| No root face or gap too wide | Burn-through, sagging root |
| Angle too narrow | Poor access, lack of sidewall fusion |
| Welding over oxide or scale | Porosity, inclusions |
| Bevel cut without kerf compensation | Part too short, wrong gap |
Fit-up checklist
- Joint dimensions per the drawing and WPS (angle, root face, root opening)
- Misalignment (hi-lo) within the procedure tolerance
- Surfaces clean and dry over the prescribed width
- Proper tacking, parts clamped to limit distortion
- Preheat if the procedure requires it (thickness, grade)
- Part identification and material traceability if required
FAQ
Who sets the angle and root face?
The drawing and the company’s qualified welding procedure; standards contain prequalified joints with their tolerances.
Should a plasma-cut edge be ground before welding?
It depends on the procedure, grade and edge condition (dross, nitriding, oxide); many procedures require at least mechanical cleaning.
Sources
- Canadian Welding Bureau (CWB Group) — CSA W47.1 certification, consulted November 26, 2026.
- CSA Group — CSA W59, Welded steel construction, consulted November 26, 2026.
- Lincoln Electric — Guide to welding pipe (PDF), consulted November 26, 2026.
- Lincoln Electric — Weld fusion vs weld penetration, consulted November 26, 2026.
One guide a week, French-first
New guides, used equipment in Quebec and price moves. No third-party ads.