Process · non-conventional machining
EDM, wire and sinker: how it works, what it’s for and its limits
EDM removes material with sparks, with no cutting force: wire for through profiles and tapers, sinker for blind cavities. Materials, recast layer, skim passes and when to choose it.
EDM (Electrical Discharge Machining) removes material with a series of sparks between an electrode and the part, in a dielectric fluid. No contact, no cutting force: material hardness barely matters, only conductivity does.
Wire or sinker?
| Criterion | Wire EDM | Sinker (ram) EDM |
|---|---|---|
| Electrode | Thin, continuously fed wire (often brass) | Electrode machined to shape (graphite or copper) |
| Dielectric | Usually deionized water | Usually dielectric oil |
| Shapes | Through profiles, tapers, punches and dies | Blind cavities, fine ribs, 3D forms, sharp inside corners |
| Start | Start hole (or part edge) | Part surface |
| Uses | Blanking dies, gears, carbide parts, fine slots | Molds, cavities, details impossible to mill |
Strengths
- Hardened materials, carbide, superalloys (see Inconel 625 and 718) machined after heat treatment.
- No burr, no force: thin or fragile parts.
- Very sharp inside corners (limited by wire diameter or electrode shape).
- Excellent precision and repeatability with skim passes.
Limits
- Slow compared with milling.
- Conductive materials only.
- Recast layer (white layer): remelted and resolidified metal at the surface, hard, sometimes cracked and stressed. Low-energy skim cuts reduce it; some specifications require it be limited or removed.
- Sinker electrodes must be made (cost, wear).
Quebec shops offering this service
- DP Digital Precision
Terrebonne, QC
Wire EDM and 5-axis CNC machining; AS9100 certified.
dpdigitalprecision.ca (opens in a new tab) - MG Metal MFG
Québec, QC
Milling, turning, wire EDM, CMM inspection and finishing.
mgmetalmfg.com (opens in a new tab) - Patt
Saint-Eustache, QC
Wire EDM, grinding, CNC milling and turning of large parts.
patt-technologies.com (opens in a new tab)
Shops are listed free of charge and in no order of preference (alphabetical). Services checked on each shop’s official website on November 26, 2026; confirm capacity and lead time before ordering.
Typical workflow (wire)
- Design the part around the start hole and tabs (so the slug doesn’t drop).
- Program the contour (wire CAM: ESPRIT, Mastercam Wire, etc.) with wire offset and number of passes.
- Clamp the part flat, align.
- Rough cut then skim passes per tolerance and finish.
- Remove tabs and finish.
Common mistakes
| Mistake | Consequence |
|---|---|
| Asking for EDM where an end mill would do | Needless cost and lead time |
| Forgetting the recast layer on a fatigue part | Crack initiation |
| No start hole planned | Extra operation |
| Specifying an inside corner sharper than the wire | Impossible on wire; sinker needed |
Checklist for subcontracting EDM
- Material and condition (hardened?) stated
- Tolerances and surface finish realistic for the process
- Recast layer requirement if critical
- Start hole provided or to be drilled by the subcontractor
- Clean 3D model or DXF (see DXF best practices)
FAQ
Can EDM cut glass or plastic?
No: the material must be conductive.
Why is wire EDM so precise?
No cutting force or significant tool wear (the wire is always fresh), plus successive skim passes.
Sources
- Makino — EDM: when milling just won’t cut it, consulted November 26, 2026.
- Makino — Wire EDM tutorial, consulted November 26, 2026.
- SME — Electrical Discharge Machining study guide (PDF), consulted November 26, 2026.
One guide a week, French-first