Materials · carbon steel
1018 cold-drawn vs hot-rolled (and A36): tolerances, residual stress and machining
1018 cold-drawn (CRS) or hot-rolled (HRS) bar, or A36: finish, tolerances, strength, residual stresses that bow parts machined on one side, case hardening and welding.
1018 (SAE/AISI, about 0.18% carbon) is the most common bar steel in machining. It’s sold mainly cold drawn / cold finished (“CRS”) and sometimes hot rolled (“HRS”). A36 is a structural standard: you find it in hot-rolled flat bar and shapes. Chemically the three are close, but not when machining.
Comparison
| Criterion | 1018 cold drawn | 1018 hot rolled | A36 hot rolled |
|---|---|---|---|
| Surface | Smooth, clean | Mill scale | Mill scale |
| Dimensional tolerances | Tight (ready-to-use bar) | Wide | Wide |
| Strength | Higher (cold work from drawing) | Lower | Specified by A36 |
| Residual stress | High | Low | Low |
| Composition | Controlled by SAE 1018 | Same | A36 mainly controls mechanical properties |
| Uses | Shafts, pins, precise machined parts | Heavily machined parts, welded parts | Structure, welded fabrication |
The trap: cold-drawing stresses
Drawing leaves internal stresses. When you remove material from one side only (keyway, pocket, asymmetric facing), the bar bows. Common fixes:
- Rough both sides, let it rest (or stress relieve thermally), then finish.
- Machine symmetrically where possible.
- Choose hot-rolled or A36 for heavily pocketed parts, or stress-relieved / ground bar.
Machining
- Cold-drawn 1018 machines decently but can be gummy (long chips); production screw machining prefers resulfurized steels (see 12L14 and 1215 (free-machining)).
- Published machinability ratings (B1112 = 100 reference): about 70–78% for 1018, per distributor tables.
- Chip breakers, adequate feed and coolant improve chip control.
Case hardening and welding
- 1018 is a classic carburizing steel: tough core, hard surface.
- It welds well; leaded or resulfurized steels weld poorly.
Common mistakes
| Mistake | Consequence |
|---|---|
| Deep keyway in cold-drawn 1018 without stress relief | Bowed shaft |
| Using A36 for a precision turned part | Extra stock to remove, abrasive scale |
| Assuming A36 = 1018 | Composition and properties not equivalent |
| Welding 12L14 instead of 1018 | Porosity, cracks |
Ordering checklist
- Grade and condition (1018 CD, 1018 HR, A36)
- Shape and size (round, square, flat, hex)
- Required tolerance (drawn vs ground/polished)
- Length and cut-to-length by the supplier
- Compare published prices in the price comparison tool
FAQ
Why is cold-drawn 1018 stronger than hot-rolled?
Cold drawing work-hardens the bar; strength rises, ductility drops a little, and internal stresses appear.
Can 1018 be through-hardened?
Not effectively: too little carbon. It’s carburized to harden the surface, or you choose an alloy steel (see 4140 vs 4340).
Sources
- Noramark — A36 vs 1018 steel, consulted November 26, 2026.
- Noramark — 1018 steel: properties, machinability, uses, consulted November 26, 2026.
- Metals Service Center Institute — Machinability ratings, consulted November 26, 2026.
One guide a week, French-first
New guides, used equipment in Quebec and price moves. No third-party ads.